CLF Workshop Floor before the makeover

CLF Team Grind the floor

CLF Dura Top 410 is applied onto the floor, with a primer placed before.

An Epoxy Primer is placed after 24 hours

2 Coats of Epoxy Screed Applied

A Sealer and Surface Hardener is Applied

The floor is ready to be used